Cold polymerizing acrylic material for the manufacturing of hard, fadeless earmolds. Free of amine and cadmium. Polymerization under pressure at a minimum of 2 bar and a maximum of 6 bar, at a temperature of 40 - 45 °C (104 - 113 °F).
Polymerization time: 12 min.
Color: transparent
Storage Temperature <30°C
Contents: 500 ml